Alloy Approx. Pouring Temp Density Characteristics
BP (Britannia Pewter) 350 °C 7.3g/cm3 Non toxic, strong, takes a high polish
92 300 °C 7.3g/cm3 Lead free, strong, good detail
KP 280 °C 7.6g/cm3 Softer than 92, good detail, low pouring temp
C 300 °C 9.3g/cm3 Soft alloy, good detail
29 320 °C 10.0g/cm3 -
20 340 °C 10.2g/cm3 -
18 solder 145 °C - Good fluidity, good wetting
HAYESOL 70 (Cerrobend) 68 °C - Good melting point alloy for fire sprinklers, pipe bending and proof pattern making
HAYESOL 11 (BS3332B) 425 °C - High load tin base bearing alloy
HAYESOL 11 (BS3332B) 480 °C - Same as above but with higher fatigue resistance
HAYESOL 12 (SAE 11) 400 °C - High strength hard tin base bearing alloy
HAYESOL 13 (DLM No.8) 370 °C - Cost effective lead base bearing alloy
HAYESOL 100 100 °C - Cadmium free fusible alloy for X-Ray shielding
UWBA (Under Water Bearing Alloy) 400 °C - For stern bearings. Alloy is equipotential to iron
Antimonial Lead - - Used for boat keels
- - -